Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay LUBRHOPHOS® LP 700 E Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name LUBRHOPHOS®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay LUBRHOPHOS® LP 700 E Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Identification: POLYOXYETHYLENE PHENYL PHOSPHATE ESTER, ACID FORM.CAS: 39464 – 70 – 5Solubility: Soluble in water and most polar and aromatic solvents.Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: Industrial formulations: Anti-wear agent and corrosion inhibitor used in water-based synthetic metalworking fluids. Low foaming hydrotrope for metal cleaning fluid. Metal treatment: Anti-wear agent and corrosion inhibitor used in water-based synthetic metalworking fluids. Low foaming propertiesInformation provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
Thermal Properties Metric English Comments
Pour Point 0.000 °C
32.0 °F
Flash Point >= 100 °C
>= 212 °F
Optical Properties Metric English Comments
Gardner Color Number <= 4.0
<= 4.0
RPG18
Chemical Properties Metric English Comments
Total Acid Number 96 - 107
96 - 107
[mg KOH/g]; RPG44
Processing Properties Metric English Comments
Moisture Content <= 1.0 %
<= 1.0 %
RPG16
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Clear to slightly hazy viscous liquid
RPG31
Composition Active
1
Nonionic content
<7%, RPG35
Ionic Charge Anionic
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved