Solvay MIRANOL® CM CONC-OP Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name MIRANOL®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay MIRANOL® CM CONC-OP Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Chemical Name: SODIUM COCOAMPHO ACETATECAS: 68608-65-1, 64-17-5Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: MIRANOL CM CONC-OP is a high foaming, mild emulsifier.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Solids Content 41 - 43 %
41 - 43 %
Moisture Balance; RP-0536
pH 12 - 13

@Temperature 30.0 °C
12 - 13

@Temperature 86.0 °F
RP-0420
Optical Properties Metric English Comments
Gardner Color Number <= 3.0
<= 3.0
RP-0138
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Composition Active
34.2-37.2%, =%Solids-%Sodium Chloride
Sodium Chloride
5.8-6.8%, RP-0097