Solvay RHODAFAC® ASI 80 BC Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay RHODAFAC® ASI 80 BC Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Identification: SOLUTION OF OCTYLPHOSPHONIC ACID IN DIETHYLENE GLYCOL MONOBUTYL ETHER AND WATER CAS : 4724 – 48 – 5 and 112 – 34 – 5Available in: Asia Pacific, Europe, Latin America and North AmericaLiquid above 30°C and Solid below 15°CSolubility: Soluble in common organic solvents and partially soluble in waterApplications: Surface treatment. Pigment dispersant. Corrosion inhibitor for metalworking formulations, cleaners and industrial applicationsInformation provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
pH 2.0
2.0
5% aqueous dispersion
Chemical Properties Metric English Comments
Total Acid Number 445 - 465
445 - 465
[mg KOH/g]; OPTI065
Processing Properties Metric English Comments
Moisture Content 8.0 - 12 %
8.0 - 12 %
OPTI074
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Color <50
Hazan, 50%, OSTMO30
Purity by 31P NMR, OPTI064
>96%