Solvay RHODAPON® ALSA/K Surfactant

Category Fluid
Manufacturer Solvay
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay RHODAPON® ALSA/K Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Chemical Name: AMMONIUM LAURYL SULFATECAS: 68081-96-9 Available in: Asia Pacific, Europe, Latin America and North America Applications: RHODAPON© ALSA/K is a primary surfactant providing excellent foaming in shampoo, body wash and bath products. Rhodapon ALSA/K is preserved with Kathon. The ammonium counterion offers improved solubility and mildness over sodium based lauryl sulfates.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
pH 6.0 - 7.0
6.0 - 7.0
10% Solution; RP-0420
Viscosity 3000 - 10000 cP
3000 - 10000 cP
LVT SSA #31 @ 3 rpm; RP-0596
Optical Properties Metric English Comments
Gardner Color Number <= 2.0
<= 2.0
RP-0138
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Clean, Clear to Hazy Viscous Liquid
RP-0064
Composition Ammonium Chloride
<0.5%, RP-0098
Anionic Active
27.5-28.5%, EQ. WT. 293, RP-0033
Disodium EDTA
>0.1%, RP-17648
Kathon
0.06-0.08%, as 1.5% Solution, RP-0281
Unsulfated Matter
<0.8%, RP-17303