Solvay RHODICARE D Surfactant

Category Fluid
Manufacturer Solvay
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay RHODICARE D Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Rhodicare® D is an anionic bio-polymer with excellent stabilizing, thickening and suspending properties. It has high electrolyte stability over a wide range of pH and fast hydration rate. It exhibits Pseudo-plastic non-thixotropic behaviour, antisyneresis agent and reduces gel exudationC.T.F.A. /I.N.C.I. Name: XANTHAN GUMCAS: 11138 - 66 – 2EINECS: 234 – 394-2Recommended use level: 0.2 - 1%Soluble in waterCompatible with Non-ionic, anionic and amphoteric surfactants.Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: Sodium salt of an anionic high molecular weight hetero-polysaccharide produced by pure culture fermentation of Xanthomonas campestris, purified by recovery with isopropanol. Thickening and stabilizing hydrocolloid giving aqueous solutions of high viscosity and high yield value even at low concentrations, not affected by temperature. Pseudo-plastic non thixotropic behaviour. Effective suspending and stabilizing agent for multi-phasic systems : aqueous suspensions, emulsions and foams, easily sprayable, flowable, pumpable (creams and lotions, toothpastes…). Thickening agent for creams, suspensions, shampoos, gels ; synergistic effect with galactomannanes, glucomannanes. Anti-syneresis agent, reduces gel exudation.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Particle Size 75 µm
75 µm
5 max, 200 mesh; TI-2087
850 µm
850 µm
90 min, 20 mesh; TI-2087
pH 6.0 - 8.0
6.0 - 8.0
1% aqueous sol.; TI-2076
Brookfield Viscosity 1200 - 1800 cP
1200 - 1800 cP
1% in 1% KCl, LVT, 60 rpm, spindle 3; TI-1110
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Granules
Color Creamy
Composition 2-Propanol
<750 ppm, TI-2105
Arsenic as As
<3 mg/kg, USP
Ash
6.5-16%, TI-0130
Cadmium (Cd)
<1 mg/kg, USP
Entero-bacteria & other Gram Neg.
Absence in 1g, TI-2101
Heavy metal as Pb
<10 mg/kg, USP
Lead as Pb
<2 mg/kg, USP
Mercury (Hg)
<1 mg/kg, USP
Pseudomonas aeruginosa
Absence in 1g, TI-2073
Staphylococcus aureus
Absence in 1g, TI-2073
Total viable aerobic count
<500 cfu/g, TI-2070
Yeasts and moulds
<100 cfu/g, TI-2071
Loss on drying 8-14%
TI-0515