Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay RHODOLINE® 643 Surfactant

Category Fluid
Manufacturer Solvay
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay RHODOLINE® 643 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description :Highly efficient mineral oil based defoamers for flat to gloss paints, quick process foam know down and high in-can persistency.Identification: OIL BASE DEFOAMERAvailable in: North AmericaApplications: RHODOLINE© 643 is a defoamer especially formulated to give outstanding foam control when used in the manufacture of paints and coatings. In paint formulations, 2 – 6 pounds of RHODOLINE© 643 will effectively defoam 100 gallons of paint, providing prolonged protection RHODOLINE© 643 is not water-dispersible and should be used as received.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 0.830 - 0.870 g/cc
0.0300 - 0.0314 lb/in³
RP-17617
Viscosity 600 - 1000 cP
600 - 1000 cP
#3 SP @ 60 rpm; RP-0596
Ash 1.5 - 2.5 %
1.5 - 2.5 %
RP-0065
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Opaque, Tan Liquid
RP-0064
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved