Solvay RHODOPOL® G Surfactant

Category Fluid
Manufacturer Solvay
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay RHODOPOL® G Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Rhodopol® G is granular and dust free grade of Xanthan Gum. It is It exhibits high pseudoplastic behavior effective thickening and stabilizing agent. It has rapid hydration properties without fish-eyes.Identification: XANTHAN GUMCAS: 11138 – 66 – 2Available in: Asia Pacific, Europe, Latin America and North America.Applications: Household liquid scaling products, Scouring creams, Alkaline oven cleaners, Industrial uses and Oilfield: Viscosifier for water-based drilling mud systems, dustless, rapid hydration without fish-eyes.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Particle Size <= 75 µm
<= 75 µm
<5%; TI-2087
<= 1180 µm
<= 1180 µm
>95%; TI-2087
pH 6.0 - 8.0
6.0 - 8.0
1% aq. Sol.; TI-2076
Brookfield Viscosity 1200 - 1600 cP
1200 - 1600 cP
1% sol. in 1% KCl Brookfield LV 60 rpm spindle n°3; TI-1110
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Granulated powder
Color Cream
Loss on drying 6-14%
TI-0515