Solvay SOPROPHOR® BSU Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name SOPROPHOR®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay SOPROPHOR® BSU Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Multipurpose dispersing agent for SC formulationsIdentification: ETHOXYLATED TRISTYRYLPHENOLCAS: 99734 – 09 – 5Solubility: Soluble in water and most polar and aromatic solvents.Available in: Asia Pacific, Europe, Latin America and North America Applications: Emulsifier, dispersing agent.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
pH 9.0 - 11
9.0 - 11
5% in water; RPG02
Thermal Properties Metric English Comments
Pour Point 15.0 °C
59.0 °F
Flash Point >= 100 °C
>= 212 °F
Processing Properties Metric English Comments
Moisture Content <= 0.50 %
<= 0.50 %
RPG16
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Viscous liquid
Composition Active
1
HLB number 12.6
Ionic Charge Nonionic
Moles of Ethylene Oxide 16