Solvay Specialty Polymers Algoflon® 15GR PTFE; Graphite Filled  (discontinued **)

Category Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Algoflon® 15GR PTFE; Graphite Filled  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer.15 wt.% Graphite. Suspension polymer powder grade recommended for compression molding. Pure PTFE possesses high inertness, excellent dielectric properties, almost no moisture absorption, low friction coefficient, and is nonflammable.
Physical Properties Metric English Comments
Density 2.17 g/cc
0.0784 lb/in³
ASTM D792
Linear Mold Shrinkage 0.021 cm/cm
0.021 in/in
Radial shrinkage of 10 cm o.d. sintered rod at 23°C
Mechanical Properties Metric English Comments
Hardness, Shore D 57
57
Tensile Strength, Ultimate 24.0 MPa
3480 psi
ASTM D638
Elongation at Break 230 %
230 %
ASTM D638
Coefficient of Friction, Dynamic 0.060
0.060
ASTM D1894
Coefficient of Friction, Static 0.080
0.080
ASTM D1894
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 190 µm/m-°C

@Temperature 23.0 - 250 °C
106 µin/in-°F

@Temperature 73.4 - 482 °F
ASTM D696
Thermal Conductivity 0.750 W/m-K
5.20 BTU-in/hr-ft²-°F
ASTM C177
Maximum Service Temperature, Air 260 °C
500 °F
Continuous Service
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+7 ohm-cm
1.00e+7 ohm-cm
ASTM D257