Material Notes:
IXAN® SGA-1 is a self-adhesive coat for use on aluminum, steel and plastic films, metalized or not. This universal grade may also be used as an adhesion primer for laminating or coating on plastic films. This resin is soluble in a wide range of solvents at room temperature.Uses: Coating ApplicationsAdditional Properties: Appearance - White powder; Density - 0.500 g/cm³; Density - 1.650 g/cm³; Heat Seal Maximum Resistance - 0.75 N/cm; Heat Seal Threshold - 115 °C; Solvents - Common solvents; Turbidity - (20°C): 77.0 µA; Viscosity - (20°C): 60 mPa·s; Volatiles - < 1.5 %Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Water Vapor Transmission 150 g/m²/day

@Thickness 0.00100 mm,
Temperature 38.0 °C
9.66 g/100 in²/day

@Thickness 0.0000394 in,
Temperature 100 °F
90% RH; ASTM F1249
Oxygen Transmission Rate 250 cc/m²/day

@Thickness 0.00100 mm
16.1 cc/100 in²/day

@Thickness 0.0000394 in
85% RH; ASTM D398
Descriptive Properties Value Comments
Agency Ratings EC 1907/2006 (REACH); EU No 10/2011
Availability Asia Pacific
Europe
North America
Color White
Form Powder