Material Notes:
Formula: CHClFCF3; Name: 1 Chloro 1,2,2,2 Tetrafluoroethane. Replaces CFC 11, 114. Refrigerant blends components for middle temperatures, polystyrene and polyethylene foams.Information provided by Solvay Solexis, Inc.
Physical Properties Metric English Comments
Density 1.36 g/cc

@Temperature 25.0 °C
0.0491 lb/in³

@Temperature 77.0 °F
Liquid
Molecular Weight 136.5 g/mol
136.5 g/mol
Vapor Pressure 3.84 bar

@Temperature 25.0 °C
2880 torr

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Heat of Vaporization 165 J/g
71.0 BTU/lb
at Boiling Point
Melting Point -198 °C
-324 °F
at 1.013 bar
Boiling Point -12.0 °C
10.4 °F
at 1.013 bar
Chemical Properties Metric English Comments
Critical Pressure 36.34 bar
27260 torr
Critical Temperature 122.5 °C
252.5 °F
Critical Density 0.560 g/cc
0.0202 lb/in³
Descriptive Properties Value Comments
Flammability Range (vol%) None
Ozone Depletion Potential 0.065
Based on CFC11 = 1.0
Toxicity Level 1000 ppm
Allowed limit in work places (values suggested by producers).