Solvay Specialty Polymers Polymist® XPP 515-S Polytetrafluoroethylene (PTFE)

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , PTFE Powder
Manufacturer Solvay Specialty Polymers
Trade Name Polymist®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Polymist® XPP 515-S Polytetrafluoroethylene (PTFE).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polymist® 515-S a white PTFE micronized powder PTFE micronized powder composed of discrete particles. Designed for use in critical engineering and high end performance plastics applications, Polymist® XPP 515-S will improve wear resistance and low coefficient of friction.Main features of Polymist® 515-S are, Improved wear resistance, Increased pressure x velocity (PV) limits, Reduced friction and stick-slip responseUses: AdditiveAdditional Properties: Bulk Density - ASTM D4895 400 g/l; Melt Temperature - ASTM D3418 320 to 330 °C; Particle Size - Internal Method 20.0 µm; Specific Surface Area - Internal Method 3.0 m²/gInformation provided by Solvay Specialty Polymers.
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
North America
Color White
Form Powder