Spartech 2850-60 PVC for Regulated Applications

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Spartech
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Spartech 2850-60 PVC for Regulated Applications.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Spartech
Physical Properties Metric English Comments
Specific Gravity 1.17 g/cc
1.17 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
Tensile Strength, Yield 11.7 MPa
1700 psi
Elongation at Break 450 %
450 %
Thermal Properties Metric English Comments
Brittleness Temperature -42.0 °C
-43.6 °F