Material Notes:
Description: Structural SheetInformation provided by Spartech.
Physical Properties Metric English Comments
Specific Gravity 1.39 g/cc
1.39 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength, Yield 73.1 MPa
10600 psi
ASTM D638
Tensile Modulus 4.044 GPa
586.6 ksi
ASTM D638
Flexural Yield Strength 93.1 MPa
13500 psi
ASTM D790
Flexural Modulus 2.53 GPa
367 ksi
ASTM D790
Falling Dart Impact 27.5 J
20.3 ft-lb
73°F; ASTM D3029
Thermal Properties Metric English Comments
CTE, linear 32.4 µm/m-°C

@Temperature 20.0 °C
18.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 138 °C
280 °F
ASTM D648
Optical Properties Metric English Comments
Gloss 90 %
90 %
Gardner; ASTM D2523