Material Notes:
Application: Extrusion for refrigerator sealsInformation provided by STIR SpA
Physical Properties Metric English Comments
Density 1.405 g/cc
0.05076 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 76
76
ISO 868
Tensile Strength at Break 15.63 MPa
2267 psi
ISO R 527
Elongation at Break 310 %
310 %
ISO R 527