Stir SpA RF 1000A (PVC)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Extruded
Manufacturer Stir SpA
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Stir SpA RF 1000A (PVC).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Application: Extrusion shock resistant profiles for windowsInformation provided by STIR SpA
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 38.0 MPa
5510 psi
ISO R 527
Elongation at Break 137 %
137 %
ISO R 527
Izod Impact, Notched 0.950 J/cm
1.78 ft-lb/in
ISO 180
Thermal Properties Metric English Comments
Vicat Softening Point 81.0 °C
178 °F
ISO 306