Stir SpA SPI 78 ATC (PVC)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Molded
Manufacturer Stir SpA
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Stir SpA SPI 78 ATC (PVC).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Application: Ecological PlugsInformation provided by STIR SpA
Physical Properties Metric English Comments
Density 1.408 g/cc
0.05087 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 77
77
ISO 868
Tensile Strength at Break 13.6 MPa
1970 psi
ISO R 527
Elongation at Break 308 %
308 %
ISO R 527
Abrasion 294
294
mm³; ISO 4649