Material Notes:
Application: Foamed intersoleInformation provided by STIR SpA
Physical Properties Metric English Comments
Specific Gravity 1.185 g/cc
1.185 g/cc
ISO 1183
Density 0.770 g/cc
0.0278 lb/in³
Foamed Density; ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 52
52
ISO 868
Tensile Strength at Break 9.66 MPa
1400 psi
ISO R 527
Elongation at Break 415 %
415 %
ISO R 527
Abrasion 141
141
Close, mm³; ISO 4649
334
334
Foam, mm³; ISO 4649