Material Notes:
Applications: STRUKTOL POLYDIS 3680 is used where conventional epoxy systems are unable to satisfy the demands of for example impact, flexural or peel strength especially at low temperatures. Significant improvements in impact strength, flexural strength, shear strength and peel strength. Largely unaffected are heat distortion temperature, chemical resistance and weathering resistance.Information provided by Struktol
Physical Properties Metric English Comments
Solids Content 80 %
80 %
in Methyl-ethyl-ketone (MEK)
Chemical Properties Metric English Comments
Acid Value <= 1.0
<= 1.0
Processing Properties Metric English Comments
Shelf Life >= 12.0 Month
>= 12.0 Month
in original sealed containers at temperatures less than 40°C
Descriptive Properties Value Comments
Appearance Yellowish, low viscous liquid
Elastomer Content % 25 NBR (in solid state)
Epoxy Equivalent Weight (g/Eq) 370
Resin-base of the prepolymer high functional Kresol-Novolac resin