Struktol VP 3742 S Flame retarded epoxy resin

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoset , Epoxy
Manufacturer Struktol
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Struktol VP 3742 S Flame retarded epoxy resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: STRUKTOL VP 3742 is a polyfunctional epoxy resin which contains a chemically bound organo-phosphorous substance. Thus the mechanical properties like stability and modulus as well as chemical resistance are not influenced negatively as it occurs when using additives or filling agents.Information provided by Struktol
Physical Properties Metric English Comments
Solids Content 80 %
80 %
Electrical Properties Metric English Comments
High Amp Arc Ignition, HAI 4.0 arcs
4.0 arcs
Processing Properties Metric English Comments
Shelf Life >= 12.0 Month
>= 12.0 Month
in original sealed containers at temperatures less than 40°C
Descriptive Properties Value Comments
Appearance Yellowish resin
Epoxy Equivalent Weight (g/Eq) 370