Styron DL 380 Carboxylated SB

Category Polymer , Thermoplastic , Styrene-Butadiene
Manufacturer Styron
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styron DL 380 Carboxylated SB.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Performance Features: Primer for hot melt PSA, barrier to PSA bleedApplications: PSAEuropeInformation provided by Styron
Physical Properties Metric English Comments
Solids Content 50 %
50 %
pH 5.0
5.0
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -8.00 °C
17.6 °F