Styron DL 395PA Modified SB

Category Polymer , Thermoplastic , Styrene-Butadiene
Manufacturer Styron
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styron DL 395PA Modified SB.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Performance Features: General purpose heat sealable, low odor, high water resistance, casein compatibility, isocyanate adhesive modifierApplications: Foil Laminated (FSK), Heat Sealable, Laminated (Metalized Paper) and Wood Adhesive (EPI)Asia PacificInformation provided by Styron
Physical Properties Metric English Comments
Solids Content 50.5 %
50.5 %
pH 6.5
6.5
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 10.0 °C
50.0 °F