Material Notes:
Overview: PULSE GX50 engineering resins give exceptional impact strength even at low temperature and have sufficient heat resistance for the majority of automotive interior components. This resin provides excellent flow, and low odor & VOC values and is self colorable.Applications: PULSE GX50 is used in a wide range of applications where low temperature toughness and tailor made heat resistance is required.Information provided by Styron
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
ISO 1183/B
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
ISO 294-4
Melt Flow 12 g/10 min

@Load 5.00 kg,
Temperature 260 °C
12 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 80.0 MPa
11600 psi
ISO 527-2
Tensile Strength, Yield 43.0 MPa
6240 psi
ISO 527-2
Tensile Modulus 2.00 GPa
290 ksi
ISO 527-2
Charpy Impact, Notched 5.00 J/cm²

@Temperature -30.0 °C
23.8 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
5.00 J/cm²

@Temperature 23.0 °C
23.8 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 93.0 °C
199 °F
Unannealed; ISO 75-2/A
Vicat Softening Point 109 °C
228 °F
ISO 306/B50
Processing Properties Metric English Comments
Melt Temperature 255 - 275 °C
491 - 527 °F
Mold Temperature 70.0 - 80.0 °C
158 - 176 °F
Descriptive Properties Value Comments
Carbon Emission 10 µg/g
VDA 277