Styron XU 31585.00 Carboxylated SB

Category Polymer , Thermoplastic , Styrene-Butadiene
Manufacturer Styron
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styron XU 31585.00 Carboxylated SB.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Performance Features: Ignition resistantApplications: Foil Laminated and Laminated (Metalized Paper)North AmericaInformation provided by Styron
Physical Properties Metric English Comments
Solids Content 50 %
50 %
pH 7.8
7.8
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 23.0 °C
73.4 °F