Material Notes:
Hiprolon® 70 NN is medium viscosity polyamide 6.10 containing a bio-renewable resource. Features: low density, low water absorption, high dimension stability, high notched impact resistance, good chemical resistance. It is widely used as a resin for further compounding, general injection molding and extrusion.Information provided by Suzhou Hipro Polymers Co. Ltd
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ISO 1183
Water Absorption 1.4 %
1.4 %
ISO 62
Mechanical Properties Metric English Comments
Tensile Strength, Yield 52.0 MPa
7540 psi
ISO 527-1/-2
Elongation at Break >= 50 %
>= 50 %
ISO 527-2/1A
Tensile Modulus 2.00 GPa
290 ksi
ISO 527-1/-2
Flexural Modulus 1.70 GPa
247 ksi
ISO 178
Charpy Impact Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179/1eU
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 0.600 J/cm²

@Temperature -30.0 °C
2.86 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
0.800 J/cm²

@Temperature 23.0 °C
3.81 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 222 °C
432 °F
ISO 11357-3