Sylvin Technologies 6134-80 PVC Wire/Cable Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Sylvin Technologies
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sylvin Technologies 6134-80 PVC Wire/Cable Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Sylvin Technologies Inc.
Physical Properties Metric English Comments
Specific Gravity 1.24 g/cc
1.24 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
10 seconds
Tensile Strength, Ultimate 15.2 MPa
2200 psi
Elongation at Break 350 %
350 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 90.0 - 105 °C
194 - 221 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Low Temperature Flexibility
Brittleness Temperature -42.0 °C
-43.6 °F
Flammability, UL94 V-1
V-1
VW-1
Oxygen Index 23.8 %
23.8 %
Processing Properties Metric English Comments
Processing Temperature 166 - 177 °C
330 - 350 °F
Recommended Stock Temperature