Information provided by Sylvin Technologies Inc.
Physical Properties Metric English Comments
Specific Gravity 1.27 g/cc
1.27 g/cc
Thickness 1000 microns
39.4 mil
Mechanical Properties Metric English Comments
Hardness, Shore A 95
95
10 seconds
Tensile Strength, Ultimate 22.1 MPa
3200 psi
Elongation at Break 310 %
310 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 50.0 °C
122 °F
RTI
Flammability, UL94 HB
HB
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Processing Properties Metric English Comments
Melt Temperature 174 - 185 °C
345 - 365 °F