Sylvin Technologies 9915-75 Natural PVC Molding Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Molded
Manufacturer Sylvin Technologies
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sylvin Technologies 9915-75 Natural PVC Molding Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Sylvin Technologies Inc.
Physical Properties Metric English Comments
Specific Gravity 1.26 g/cc
1.26 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
10 seconds
Tensile Strength, Ultimate 15.2 MPa
2200 psi
Elongation at Break 430 %
430 %
Tear Strength Test 310
310
Processing Properties Metric English Comments
Melt Temperature 163 - 174 °C
325 - 345 °F