Synergy Polymers Ultra Purge PET-E

Category Polymer , Thermoplastic , Purging Compound
Manufacturer Synergy Polymers
Trade Name Ultra Purge
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Synergy Polymers Ultra Purge PET-E.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Best with color changes. Cleans out barrels, nozzles and heads of extruders from carbon remnants and removes black specs, deposits and incrustations. Specifically designed for the production of preforms and containers for the food industry. For use with: Injection Molding Machines Extruders Blow Molding Machines without accumulators Purged Resin: Specifically designed for PETInformation provided by Synergy Polymers.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 320 °C
608 °F
Minimum Service Temperature, Air 190 °C
374 °F