Material Notes:
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all production and processing stages, strict final inspection, and clearly defined development processes.TIMREX Primary Synthetic Graphite shows unique properties thanks to the combination of a consistent purity, perfect crystalline structure and well defined texture.Information provided by TIMCAL
Physical Properties Metric English Comments
Bulk Density 0.0900 g/cc
0.00325 lb/in³
Scott
Particle Size 22 µm
22 µm
d90
Specific Surface Area 8.0 m²/g
8.0 m²/g
BET
Ash 0.030 %
0.030 %
Typical
Descriptive Properties Value Comments
Aspect Fine black powder
Battery type High-drain AA, AAA
Graphite 5-6%
Recommended concentration
Particle Shape Strongly anisometric, flakes