Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 1.0 PHR Thanecure ZM

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer TSE Industries, Inc
Trade Name Millathane®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 1.0 PHR Thanecure ZM.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Millathane 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and many other high performance polyurethane applications. Millathane 76 can be vulcanized by sulfur or peroxide cured systems. Thanecure ZM is an activator for a sulfur cure of Millathane® millable polyurethanes consisting of a partial complex of zinc chloride and MBTS.All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 69
69
Tensile Strength, Yield 34.45 MPa
4996 psi
Elongation at Yield 593 %
593 %
100% Modulus 0.00354 GPa
0.513 ksi
200% Modulus 0.008039 GPa
1.166 ksi
300% Modulus 0.01397 GPa
2.026 ksi
Tear Strength 62.2 kN/m
355 pli
Die C
Compression Set 24.8 %

@Temperature 70.0 °C,
Time 79200 sec
24.8 %

@Temperature 158 °F,
Time 22.0 hour
Processing Properties Metric English Comments
Cure Time 7.00 min

@Temperature 155 °C
0.117 hour

@Temperature 311 °F
TC90
Users viewing this material also viewed the following: