Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.0 PHR MBT

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer TSE Industries, Inc
Trade Name Millathane®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.0 PHR MBT.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and many other high performance polyurethane applications. Millathane 76 can be vulcanized by sulfur or peroxide cured systems.The combination of thiazole accelerators, MBTS and MBT, enable the best possible cure for Millathane® 76. An increase in MBTS results in a higher state of cure and increased processing safety.An increase in MBT decreases scorch time and increases the state of cure.All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 68
68
Tensile Strength, Yield 32.5 MPa
4710 psi
Elongation at Yield 550 %
550 %
100% Modulus 0.00362 GPa
0.525 ksi
200% Modulus 0.00827 GPa
1.20 ksi
300% Modulus 0.0147 GPa
2.13 ksi
Tear Strength 63.0 kN/m
359 pli
Die C
Compression Set 34.5 %

@Temperature 70.0 °C,
Time 79200 sec
34.5 %

@Temperature 158 °F,
Time 22.0 hour
Processing Properties Metric English Comments
Cure Time 3.40 min

@Temperature 155 °C
0.0567 hour

@Temperature 311 °F
ts2
8.20 min

@Temperature 155 °C
0.137 hour

@Temperature 311 °F
TC90