TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Non-Black, Soft Clay

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer TSE Industries, Inc
Trade Name Millathane®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Non-Black, Soft Clay.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and many other high performance polyurethane applications. Millathane 76 can be vulcanized by sulfur or peroxide cured systems.FormulationMillathane 76 100.0Zinc Stearate0.5Poly AC 617A1.0MBTS4.0MBT2.0Thanecure® ZM1.0TP-9510.0Sulfur2.0Soft Clay20All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 50
50
Tensile Strength, Yield 26.92 MPa
3905 psi
Elongation at Yield 677 %
677 %
100% Modulus 0.00136 GPa
0.197 ksi
200% Modulus 0.00234 GPa
0.340 ksi
300% Modulus 0.00358 GPa
0.519 ksi
Tear Strength 43.4 kN/m
248 pli
Taber Abrasion, mg/1000 Cycles 14

@Load 1.00 kg
14

@Load 2.20 lb
H-18 wheel
Compression Set 45.1 %

@Temperature 70.0 °C,
Time 79200 sec
45.1 %

@Temperature 158 °F,
Time 22.0 hour
Processing Properties Metric English Comments
Cure Time 10.0 min

@Temperature 155 °C
0.167 hour

@Temperature 311 °F