TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane, Hardness 52A

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane, Hardness 52A.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear strength, oil and fuel resistance, and ozone resistance. The life expectancy of urethane is often 5 times longer than other elastomers, thus saving material costs and downtime expense. One shortcoming of polyurethanes is loss of physical properties at temperatures over 180°F (82°C). MILLATHANE HT has overcome this weakness.Carbon Black with Peroxide Cure SystemFormulationMillathane HT100.0N-330 Black20.0Di-Cup 40C1.0All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 52
52
Tensile Strength, Yield 21.29 MPa
3088 psi
Elongation at Yield 493 %
493 %
100% Modulus 0.00138 GPa
0.200 ksi
200% Modulus 0.00344 GPa
0.499 ksi
300% Modulus 0.007846 GPa
1.138 ksi
Tear Strength 31.0 kN/m
177 pli
Die C
Processing Properties Metric English Comments
Cure Time 10.0 min

@Temperature 171 °C
0.167 hour

@Temperature 340 °F