Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES Electrablend® PA12 CB

Category Polymer , Thermoplastic , Nylon , Nylon 12
Manufacturer Techmer ES
Trade Name Electrablend®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Electrablend® PA12 CB.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsAdditive: Carbon BlackFeatures: ConductiveAppearance: BlackTPCI# 9874105Information provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792
Water Absorption 0.23 %

@Time 86400 sec
0.23 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0090 cm/cm

@Thickness 3.17 mm
0.0090 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 48.3 MPa
7000 psi
ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Flexural Strength 77.9 MPa
11300 psi
ASTM D790
Flexural Modulus 1.76 GPa
255 ksi
ASTM D790
Izod Impact, Notched 0.694 J/cm

@Thickness 3.17 mm
1.30 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 12.6 µm/m-°C
7.00 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 100 ohm-cm
100 ohm-cm
ASTM D257
Surface Resistance 1000 ohm
1000 ohm
ASTM D257
Users viewing this material also viewed the following: