Material Notes:
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Graphite Powder Lubricant and UV StabilizerFeatures: Heat Stabilized. Good UV Resistance and LubricatedAppearance: Natural ColorInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
ASTM D792
Water Absorption 0.20 %

@Time 86400 sec
0.20 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.015 cm/cm

@Thickness 3.17 mm
0.015 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 108
108
ASTM D785
Tensile Strength, Yield 62.1 MPa
9000 psi
ASTM D638
Elongation at Break 10 %
10 %
ASTM D638
Flexural Strength 75.8 MPa
11000 psi
ASTM D790
Flexural Modulus 1.10 GPa
160 ksi
ASTM D790
Izod Impact, Notched 0.747 J/cm

@Thickness 3.17 mm
1.40 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 126 µm/m-°C
70.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 45.0 °C
113 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 23.9 °C
75.0 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
ASTM D257
Dielectric Strength 17.7 kV/mm
450 kV/in
Method A (Short-Time); ASTM D149