Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES HiFill® PEEK GF10 10% Glass Filled

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Glass Fiber Filled
Manufacturer Techmer ES
Trade Name HiFill®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill® PEEK GF10 10% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.39 g/cc
0.0502 lb/in³
ASTM D792
Water Absorption 0.15 %

@Time 86400 sec
0.15 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0080 cm/cm

@Thickness 3.17 mm
0.0080 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength, Yield 124 MPa
18000 psi
ASTM D638
Elongation at Break 4.5 %
4.5 %
ASTM D638
Flexural Strength 153 MPa
22200 psi
ASTM D790
Flexural Modulus 5.31 GPa
770 ksi
ASTM D790
Izod Impact, Notched 0.854 J/cm

@Thickness 3.17 mm
1.60 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 28.8 µm/m-°C
16.0 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Strength 17.7 kV/mm
450 kV/in
Method A (Short-Time); ASTM D149
Users viewing this material also viewed the following: