Teknor Apex APEX® 586 Polyvinyl Chloride, Flexible

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade , PVC, Wire and Cable Grade
Manufacturer Teknor Apex Company
Trade Name APEX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex APEX® 586 Polyvinyl Chloride, Flexible.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Notes: 60°C Insulation; RoHS Compliant Uses: Tubing; Wire JacketingForms: Pellets Wire Types: SPT-1; SPT-2 Agency Ratings: UL 498; UL 62 Processing Method: Injection Molding Additional Information: Speaker Wire Temperature Rating: 60°C Ultimate Elongation Retained, UL 1581, Oven Aged, 7 days, 100°C: 77% Tensile Strength Retained, UL 1581, Oven Aged, 7 days, 100°C: 108%Information Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 85
85
15 seconds; ASTM D2240
Tensile Strength at Break 19.0 MPa
2750 psi
ASTM D638
Elongation at Break 350 %
350 %
ASTM D638
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 50.0 °C
122 °F
Continuous Use; ASTM D794
Brittleness Temperature -29.0 °C
-20.2 °F
ASTM D746
Oxygen Index 24 %
24 %
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity 3.00e+11 ohm-cm
3.00e+11 ohm-cm
ASTM D257
Descriptive Properties Value Comments
Appearance Opaque