Teknor Apex APEX® 90-P513A-75-NT Polyvinyl Chloride+PUR

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Teknor Apex Company
Trade Name APEX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex APEX® 90-P513A-75-NT Polyvinyl Chloride+PUR.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Forms-PelletsInformation provided by Teknor Apex Company
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
23°C; ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
ASTM D2240
Tensile Strength, Yield 18.6 MPa
2700 psi
ASTM D412
Elongation at Break 530 %
530 %
ASTM D412