Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Teknor Apex Flexalloy® 9800-40 Polyvinyl Chloride Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Teknor Apex Company
Trade Name Flexalloy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Flexalloy® 9800-40 Polyvinyl Chloride Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Oil Resistant, Ultra High MWUses- Footwear, Tubing, Gaskets, Tools (Power/Others), Hose, Wire and Cable Applications, SealsForms-PelletsProcessing- ExtrusionInformation provided by Teknor Apex Company
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
23°C; ASTM D792
Melt Flow 7.0 g/10 min

@Load 5.00 kg,
Temperature 177 °C
7.0 g/10 min

@Load 11.0 lb,
Temperature 351 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 40
40
15 seconds; ASTM D2240
Tensile Strength, Yield 4.59 MPa
665 psi
ASTM D412
9.17 MPa
1330 psi
200% Retention; Oil Immersion, ASTM #3 oil, 125°C, 7 days
Elongation at Break 310.4 %
310.4 %
97% Retention; Oil Immersion, ASTM #3 oil, 125°C, 7 Days
320 %
320 %
ASTM D412
Compression Set 34 %
34 %
158°F, 22 hr.; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 205 °C
401 °F
>60 min.
Brittleness Temperature -54.0 °C
-65.2 °F
ASTM D746
Descriptive Properties Value Comments
Swell 3%; Oil Immersion, ASTM #3 oil, 125°C, 7 days
Users viewing this material also viewed the following: