Material Notes:
Notes: RoHS Compliant Availability: Asia Pacific Features: Food Contact AcceptableUses: Shrink Wrap Forms: Pellets Processing Method: Blown FilmInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.34 g/cc
1.34 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 41.2 MPa
5970 psi
9.8 in/min; ASTM D638
Elongation at Break 180 %
180 %
9.8 in/min; ASTM D638
Izod Impact, Notched 1.17 J/cm
2.20 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 72.2 °C
162 °F
ASTM D1525