Teknor Apex Telcar® OBC 2419B Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV)
Manufacturer Teknor Apex Company
Trade Name TELCAR®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Telcar® OBC 2419B Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Notes: Telcar OBC has superior mechanical strength and higher elongation which will provide a tougher more durable finished product. Telcar OBC can be used in less demanding sealing applications. TPV offers a lower compression set and therefore superior sealing properties. Extrusion die swell is likely to be different from TPV's due to different chemistries used. Compounds supplied in natural color or black. Precoloring is available upon request.Information Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 0.970 g/cc
0.970 g/cc
ASTM D792
Melt Flow 0.300 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.300 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
ASTM D2240
Tensile Strength 6.55 MPa
950 psi
ASTM D412
Elongation at Break 545 %
545 %
ASTM D412
Compression Set 24 %

@Temperature 22.8 °C,
Time 79200 sec
24 %

@Temperature 73.0 °F,
Time 22.0 hour
ASTM D395B
43 %

@Temperature 70.0 °C,
Time 79200 sec
43 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D395B