Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Teknor Apex Uniprene® 50D Polyvinyl Chloride, Flexible

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade
Manufacturer Teknor Apex Company
Trade Name UNIPRENE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Uniprene® 50D Polyvinyl Chloride, Flexible.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: High Elastic RecoveryInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 0.930 g/cc
0.930 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 50
50
5 seconds; ASTM D2240
Tensile Strength at Break 22.8 MPa
3300 psi
ASTM D412
Elongation at Break 600 %
600 %
ASTM D412
100% Modulus 0.0145 GPa
2.10 ksi
ASTM D412
Tear Strength 114 kN/m
650 pli
Die C; ASTM D624
Compression Set 45 %

@Temperature -5.00 °C,
Time 79200 sec
45 %

@Temperature 23.0 °F,
Time 22.0 hour
Method B; ASTM D395
67 %

@Temperature 21.1 °C,
Time 79200 sec
67 %

@Temperature 70.0 °F,
Time 22.0 hour
Method B; ASTM D395
80 %

@Temperature 37.8 °C,
Time 79200 sec
80 %

@Temperature 100 °F,
Time 22.0 hour
Method B; ASTM D395