Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Total PPH 3480Z Polypropylene, Extrusion Grade

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Extrusion Grade
Manufacturer Total Atofina
Trade Name PPH
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total PPH 3480Z Polypropylene, Extrusion Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Homopolymer Profile Extrusion GradeProcess Stability --FINA 3480Z is formulated specifically to give excellent process stability in high profile extrusion.High Purity - Low catalyst residues in FINA 3480Z provide outstanding color, plus low taste and odor.Antistat - FINA 3480Z is formulated to minimize surface static build-up.FDA - FINA 3480Z complies with all applicable FDA regulations for food contact applications.Recommended Applications - FINA 3480Z is recommended for high speed profile extrusion for standard and flexible drinking straws.Processing - FINA 3480Z processes on conventional extrusion equipment with typical melt temperatures of 390-450°F (200-232°C)Data provided by the manufacturer, Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM D1505
Melt Flow 4.8 g/10 min
4.8 g/10 min
ASTM D1238L
Mechanical Properties Metric English Comments
Hardness, Rockwell R 90
90
ASTM D288A
Hardness, Shore D 77
77
ASTM D1706
Tensile Strength, Ultimate 35.6 MPa
5160 psi
ASTM D638
Elongation at Break >= 100 %
>= 100 %
ASTM D638
Elongation at Yield 10 %
10 %
ASTM D638
Modulus of Elasticity 1.515 GPa
219.7 ksi
ASTM D638
Flexural Modulus 1.38 GPa
200 ksi
ASTM D790
Izod Impact, Notched 0.265 J/cm
0.496 ft-lb/in
ASTM D256A
Izod Impact, Unnotched 12.7 J/cm
23.8 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
CTE, linear 100 µm/m-°C

@Temperature 20.0 °C
55.6 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Melting Point 165 °C
329 °F
DSC
Deflection Temperature at 0.46 MPa (66 psi) 107 °C
225 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 200 - 232 °C
392 - 450 °F
Extrusion
Users viewing this material also viewed the following: