Material Notes:
TRA-COAT WCC2B is a clear, medium viscosity compound developed for optical fiber, glass, and general purpose bonding. This one-part liquid cures with exposure to UV light at 100 fpm under a 300 watt/inch bulb. TRA-COAT WCC2B makes strong bonds to clear plastics and glass, and is easy to apply. Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Viscosity 21000 cP
21000 cP
Mixed (SSA #14/6R, 10 rpm)
Mechanical Properties Metric English Comments
Hardness, Shore D 75
75
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 38.0 °C
100 °F
Ultimate Tg
Descriptive Properties Value Comments
Color Clear
Cured
Clear
Adhesive