Material Notes:
Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE.
Physical Properties Metric English Comments
Mooney Viscosity 54.2

@Temperature 100 °C
54.2

@Temperature 212 °F
ML1+4; ASTM D1646
Mechanical Properties Metric English Comments
Tensile Strength at Break 0.480 MPa
69.6 psi
Elongation at Break 1290 %
1290 %
Modulus of Elasticity 0.000230 GPa
0.0334 ksi
600% Modulus
50% Modulus 0.000220 GPa
0.0319 ksi
300% Modulus 0.000200 GPa
0.0290 ksi
Thermal Properties Metric English Comments
Shrinkage 44 %
44 %
Mill Shrinkage
Processing Properties Metric English Comments
Extrusion Rate 74.5 g/min
74.5 g/min
Cure Time 10.1 min
0.168 hour
t10
12.6 min
0.210 hour
t90
Descriptive Properties Value Comments
Die Swell 4.32 g/min