Material Notes:
Fiberfrax Fibermat is a lightweight, high-strength needled insulating blanket. The blanket fibers are spun from a ceramic composition having a normal use limit of 760°C (1400°F). Fibermat is completely inorganic and derives its exceptional strength from the needling of long ceramic fibers. It has excellent thermal and acoustical insulating properties.Typical ApplicationsAcoustical insulationThermal insulation for external applicationsInsulating padsInformation Provided by Unifrax I LLC
Physical Properties Metric English Comments
Specific Gravity 2.73 g/cc
2.73 g/cc
Density 0.0881 g/cc
0.00318 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Yield 0.0483 - 0.0689 MPa
7.00 - 10.0 psi
ASTM 686-76
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 677 °C
1250 °F
Recommended Operating Temperature
Component Elements Properties Metric English Comments
Al2O3 29 - 47 %
29 - 47 %
SiO2 52 - 57 %
52 - 57 %
ZrO2 <= 18 %
<= 18 %
Descriptive Properties Value Comments
Color White
Fiber Diameter (microns) 2.5-3.5
Leachable Chlorides (ppm) <10
Na2O3 (%) <0.5
Temperature Grade (°C) 760