Unifrax Fiberfrax® PH Blanket Ceramic Fiber Insulator

Category Ceramic , Oxide , Aluminum Oxide , Silicon Oxide
Manufacturer Unifrax I LLC
Trade Name Fiberfrax®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Unifrax Fiberfrax® PH Blanket Ceramic Fiber Insulator.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fiberfrax PH blanket is a unique product that has been specifically designed to provide excellent filtration capabilities in addition to the high chemical stability and low thermal conductivity that is possessed by all Fiberfrax products.PH blanket is made from Fiberfrax bulk ceramic fibers in a unique wet felting process which removes unfiberized particles. In addition to the strength and resiliency afforded by the interlocking of fibers during the manufacturing process, handling strength is further enhanced by the addition of a small amount of organic binder.A typical filtration application would involve utilizing PH blanket as a platinum catalyst recovery filter in nitric acid production. In this application, PH blanket offers numerous advantages over glass woll products including longer life, 50-60% improved filter efficiency, reduced chance of blowouts, and better temperature resistance.Typical ApplicationsCatalyst recovery filter in nitric acid productionDiffusion medium for fluidized bedsFiltration and catalyst carrier medium for radioactive particles and hot exhaust gasesInformation Provided by Unifrax I LLC
Physical Properties Metric English Comments
Density 0.0961 g/cc
0.00347 lb/in³
Thermal Properties Metric English Comments
Melting Point 1790 °C
3250 °F
Maximum Service Temperature, Air 1177 °C
2151 °F
Recommended Operating Temperature
Component Elements Properties Metric English Comments
Al2O3 43 - 47 %
43 - 47 %
SiO2 53 - 55 %
53 - 55 %
Descriptive Properties Value Comments
Binder Content (%) 3-5
Color Tan
Fiber Diameter (microns) 4-8
Leachable Chlorides (ppm) <10
Na2O3 (%) <0.5
Temperature Grade (°C) 1260