Material Notes:
Applications include injection molding and fibers. Basic and anti-gasfading stabilization. Homopolymer.Information provided by Unipetrol RPA
Physical Properties Metric English Comments
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 36.0 MPa
5220 psi
ISO 527
Elongation at Break >= 100 %
>= 100 %
ISO 527
Flexural Modulus 1.65 GPa
239 ksi
ISO 178
Charpy Impact, Notched 0.300 J/cm²

@Temperature 23.0 °C
1.43 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 58.0 °C
136 °F
ISO 75
Vicat Softening Point 156 °C
313 °F
ISO 306