Valley Adhesives EM-120 High Performance Application Glue Stick

Category Polymer , Adhesive , Thermoset
Manufacturer Valley Adhesives
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Valley Adhesives EM-120 High Performance Application Glue Stick.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Valley Adhesives EM-120 High Performance Application Glue StickGeneral purpose hot melt spray adhesive; High performance and heat resistance with excellent adhesion, shear, peel and high initial strength; High adhesion bonding on most substrates including open cell foam and polyolefins.
Physical Properties Metric English Comments
Viscosity 3187 cP
3187 cP
Mechanical Properties Metric English Comments
Hardness, Shore A 72
72
Tensile Strength, Ultimate 1.62 MPa
235 psi
Elongation at Break 705 %
705 %
Shear Strength 2.50 MPa
363 psi
Peel Strength 5.78 kN/m
33.0 pli
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 82.2 °C
180 °F
Heat Resistance Value at 2 psi.
Softening Point 300 °C
572 °F
Processing Properties Metric English Comments
Pot Life 5.00 min
5.00 min
Open Time
Descriptive Properties Value Comments
Color Amber